Does FGD gypsum need a dryer, and how dry should it be? Often only a little drying is needed, and the dryer must not calcine it. Gypsum from a power plant’s vacuum belt filter typically carries 10–15% free moisture. CPCB guidance suggests up to 8% free moisture (measured at 45 °C) for cement plants, and under 10% for gypsum board. Taking 20 t/h of cake from 14% to 8% removes about 1.3 t/h of water. The real design limit is product temperature: overheat the dihydrate and you make hemihydrate, which can cause false set in cement. This guide is for power utilities, cement plants, gypsum traders and board manufacturers.
Moisture here means free (surface) moisture on a wet basis, unless stated otherwise. It does not include the chemically bound water inside gypsum crystals.
Why is FGD gypsum handling a live question in 2026?
Utilities with operating flue gas desulphurisation (FGD) units are now looking for regular buyers, while the expected national supply has shrunk. That makes quality, moisture and logistics decisive in each offtake deal.
- An expression of interest from NTPC Vidyut Vyapar Nigam (ref. NVVN/CandM/2025-26/RE-478, digitally signed 12 December 2025) offers FGD gypsum from NTPC stations “as is where is”, with a quality range of 85–90% minimum purity, 10–15% maximum moisture and 100–200 ppm maximum chlorides (EOI PDF).
- Mahagenco’s EOI dated 6 November 2026 invites proposals for a cement or clinker grinding unit at Koradi TPS, with fly ash support and FGD gypsum “on chargeable basis” (Mahagenco EOI). It is an information-gathering exercise, not a contract.
- On the supply side, the Environment Ministry’s notification of 11 July 2025 exempted most coal units from SO₂ norms. The Hindu reported that about 78% of coal plants were exempted from installing FGD systems.
What moisture and quality do FGD gypsum buyers ask for?
Cement plants and board makers set different limits, and the drying target should come from the buyer’s specification. CPCB’s February 2023 guidelines on FGD gypsum give the figures below. They also note that FGD gypsum is a grey, fine powder with 10–15% moisture and 80–90% calcium sulphate dihydrate.
| Use | Free moisture | Other key limits | Source |
|---|---|---|---|
| Cement (set retarder) | Up to 8%, measured at 45 °C | pH > 5; CaSO₄·2H₂O > 70%; soluble P₂O₅ < 0.5% (may be relaxed by the cement plant) | CPCB guidelines, 2023 |
| Gypsum board (preferred) | < 10% | CaSO₄·2H₂O > 95%; low chloride | CPCB guidelines, 2023 |
| FGD plant design target | ≤ 10% from the dewatering system | Chloride < 100 ppm; purity ≥ 90% | CEA standard technical specification, as quoted by CPCB |
Read the full CPCB Guidelines for Handling and Management of FGD Gypsum and refer to IS 12679 for by-product gypsum in plaster, blocks and boards. Drying does not remove chlorides; CPCB points to washing for that.
Why must an FGD gypsum dryer keep the product cool?
Gypsum is a hydrate. Pure CaSO₄·2H₂O contains 20.9% chemically bound water. Heat it too far and it loses part of that water to become hemihydrate. A VDZ study in ZKG cites dehydration to hemihydrate between 95 and 170 °C, notes that it can begin below 70 °C, and explains that too much hemihydrate leads to false setting in cement.
Cement mills already dehydrate part of the gypsum on purpose, so the cement plant needs to control that step itself. A dryer upstream should remove free water and nothing more. In practice:
- Control on product (or exhaust) temperature, not only on inlet gas temperature. Wet particles sit near the wet-bulb temperature; the risk comes once they are dry.
- Agree a maximum product temperature with the buyer and confirm it in trials by measuring combined water before and after the dryer.
- Avoid over-drying. Taking the product far below the buyer’s limit gains nothing and raises the chance of dehydration.
- Avoid hot spots and long hold-ups, such as material lying in the dryer during stoppages.
How much water does the dryer remove? A worked example
For 20 t/h of belt-filter cake at 14% free moisture dried to the 8% cement limit, the dryer removes about 1.3 t/h of water and delivers about 18.7 t/h of product. The calculation is: dry solids = 20 × 0.86 = 17.2 t/h; product = 17.2 ÷ 0.92 = 18.7 t/h; water = 20 − 18.7 = 1.3 t/h.
| Item | 14% → 8% (cement) | 14% → 5% |
|---|---|---|
| Product output | 18.7 t/h | 18.1 t/h |
| Water evaporated | 1.3 t/h | 1.9 t/h |
| Heat at an assumed 3.6 MJ/kg water | ≈ 4.7 GJ/h (≈ 1.3 MW) | ≈ 6.8 GJ/h (≈ 1.9 MW) |
| Heat per tonne of product | ≈ 0.25 GJ/t | ≈ 0.38 GJ/t |
The 3.6 MJ per kg of water is an illustrative overall figure for a direct-fired dryer including losses; use the supplier’s guaranteed value. Two lessons follow. First, drying to 8% cuts the mass shipped by only about 6.5%, so freight savings alone rarely justify a dryer. The case usually rests on meeting a buyer’s limit, stopping sticky cake from blocking chutes and hoppers, and storing it without caking. Second, going below the buyer’s limit needs about 45% more heat and adds calcination risk.
Which dryer type fits FGD gypsum?
FGD gypsum is a fine cake, so the choice is mostly between a flash dryer and a rotary dryer, with belt dryers for sticky cake.
| Dryer | Fits | Watch-outs |
|---|---|---|
| Flash dryer | Fine powder and filter cake; seconds of residence, so little time at temperature | Needs cake disintegration and good feed control; large dust collection |
| Rotary dryer | High-capacity continuous duty, coarser natural gypsum and mixed feed | Longer residence; control product temperature carefully |
| Fluid bed dryer | Granular gypsum with uniform particle size | Very fine cake may not fluidise well |
| Belt dryer | Sticky, slurry-derived cake at gentle temperatures | Larger footprint; feed must be formed into an even bed |
GTI’s gypsum dryers page covers natural and synthetic (FGD) gypsum and lists these four types, describing rotary dryers as the most widely used and flash dryers for fine powder and filter cake. It states gypsum moisture of 5% to 25% or higher depending on source, and stresses controlled drying to avoid overheating. See also GTI’s flash dryer and rotary drum dryer pages.

Which testing mistake makes a gypsum dryer look wrong?
Measuring moisture at too high a temperature. A moisture balance or oven set at 105 °C or more can drive off crystal water as well as free water, so a perfectly dried sample reads wet. CPCB specifies free moisture at 45 °C for cement use. A two-step laboratory test is often used to separate the two: free water at about 50 °C, then crystal water at 200 °C, from which purity can be calculated. Eurogypsum criteria for FGD gypsum include free moisture below 10% and dihydrate above 95%. Write the test method, temperature and sampling point into the dryer’s performance guarantee.
Frequently asked questions
CPCB describes FGD gypsum as a fine grey powder with 10–15% moisture, and NTPC’s December 2025 EOI quotes a maximum moisture range of 10–15%. The CEA technical specification for FGD systems targets no more than 10%.
Yes, if it overheats the product. Dihydrate gypsum loses crystal water to form hemihydrate at elevated temperatures, and too much hemihydrate can cause false set in cement. A dryer for cement-grade gypsum should remove free water only.
No. Chlorides stay with the solids when water evaporates. CPCB guidance points to washing the gypsum, typically on the filter, to reduce chloride, which matters most for gypsum board.
CPCB’s 2023 guidelines suggest free moisture up to 8%, measured at 45 °C, with pH above 5 and dihydrate above 70%, and note that cement plants may relax these limits. Agree the figure and test method with each buyer.
About Genex Tech Industries LLP (GTI Group)
Genex Tech Industries LLP (GTI Group) designs and manufactures flash, rotary, fluid bed and belt dryers, including the gypsum drying systems described on gtidryers.com. On this site, see our rotary dryer page, our comparison of rotary drum and flash dryers and our silica sand dryer guide for another mineral case. The head office is at 10C Middleton Row, Kolkata 700071, India.
Sources and authorship
- Central Pollution Control Board, “Guidelines for Handling and Management of Flue Gas Desulfurization (FGD) Gypsum”, February 2023 (quoting the CEA standard technical specification for wet limestone FGD).
- NTPC Vidyut Vyapar Nigam, EOI for FGD gypsum end users and traders, ref. NVVN/CandM/2025-26/RE-478, signed 12 December 2025.
- Mahagenco, EOI for a cement plant or clinker grinding unit at Koradi TPS, 6 November 2026.
- The Hindu, report on the Environment Ministry’s SO₂ notification of 11 July 2025.
- VDZ, “Gypsum dehydration potential and mean residence time of a stirred media mill…”, ZKG International.
- Published gypsum, flash and rotary dryer pages of Genex Tech Industries LLP (GTI Group).
The heat figures are an illustrative calculation from stated assumptions, not a measurement or quotation from any plant. This article was prepared by the editorial team of Genex Tech Industries LLP (GTI Group) with AI editorial assistance. It has not been reviewed by a named engineer, and no individual is cited as having approved the technical content.
Next step
Evaluating FGD gypsum drying for cement or board offtake? Email mktg@gtidryers.com or use the contact page. Send the cake moisture range and particle size, required free moisture and test method, buyer’s maximum product temperature, throughput in t/h, available heat source and the installation location.